The country of origin of a lithium-ion pouch cell
No revocation or modification of this ruling appears in the Customs Bulletin issues read here (Nov 6, 2024 through Nov 18, 2026), where CBP publishes most such actions. That is not confirmation that the ruling is still in effect. Confirm its status with CBP before relying on it (ruling on CBP CROSS).
Ruling text
In your letter dated March 28, 2025, you requested a country of origin ruling. The merchandise under consideration is referred to as an Energy Storage System lithium iron phosphate pouch cell (ESS LFP). It is described as a rectangular rechargeable lithium-ion pouch cell with a nominal voltage of 3.21 VDC, a minimum capacity of 58.7 Ah, and a minimum energy of 188 Wh. The cell measures approximately 310 millimeters in length, 110 millimeters in width, and 14.5 millimeters in thickness.
You presented two manufacturing scenarios with identical operational production steps. The only difference between the two scenarios will be the origins of the materials. The materials will be shipped to South Korea in different material forms, including in material rolls, in powder form, or as liquids shipped in bulk containers. In the first scenario, the materials are sourced from China, France, Japan, Malaysia, South Korea, and the United States.
These include cathode and anode active material sourced from China; terminal tabs, raw material for the conductor, various binder materials, rolls of separator material, and drums of electrolyte sourced from South Korea; rolls of anode foil sourced from Malaysia; rolls of film material for the pouch sourced from Japan; and binder material sourced from France or the United States. In the second scenario, the materials are sourced from China, South Korea, and the United States.
These include cathode and anode active material, various binder materials, containers of solvents, rolls of separator material, rolls of anode foil, rolls of film material for the pouch, and drums of electrolyte sourced from China; various binder materials and terminal tabs sourced from South Korea; and binder material sourced from the United States. The manufacturing process for the ESS LFP pouch cell will occur in South Korea in a partially automated production line that is divided into three sections.
The first section is dedicated to manufacturing the electrodes and begins with milling and mixing raw materials (e.g., active materials, conductive agents, solvents, and binders) to produce a slurry. The slurry is applied to a foil, creating a semi-finished roll that is subsequently flattened to the required thickness by a rolling press. Afterward, the roll is slit to the required width and stored as a semi-finished reel.
The next section involves assembling the electrode, separators, various other components, and adding electrolyte. The first step is notching, which is described as cutting the semi-finished electrode reel into sheets specific to the shape and size of the battery cell. Next, the electrode sheets are placed in a high-temperature vacuum environment to remove any moisture.
The process continues with “stacking,” a process where the anode and cathode electrode sheets are alternately stacked with separators to form a jelly roll. The final steps of this section involve welding tabs to the jelly roll, placing the roll inside a pouch, adding electrolyte, and sealing the pouch. The last section is dedicated to the formation process. The purpose of this step is to activate and verify the performance of the battery cell.
The text above is an excerpt. The official ruling, with its letterhead, signature and any attachments, is on CBP CROSS (N347172).