The country of origin of a battery cell
No revocation or modification of this ruling appears in the Customs Bulletin issues read here (Nov 6, 2024 through Nov 18, 2026), where CBP publishes most such actions. That is not confirmation that the ruling is still in effect. Confirm its status with CBP before relying on it (ruling on CBP CROSS).
Ruling text
In your letter dated July 5, 2025, you requested a country of origin ruling on behalf of your client, Sunwoda Automotive Energy Technology (Thailand) Co., Ltd. The merchandise under consideration is identified as a lithium polymer prismatic battery cell, model number SBP-01-3140, with a rigid aluminum housing that is rectangular in shape. The subject battery cell will have a nominal voltage of 3.2 VDC, a nominal capacity of 314 Ah, and a nominal energy of 1005 Wh.
Its dimensions are approximately 174.3 millimeters in width, 206.9 millimeters in height, and 71.5 millimeters in thickness. The subject prismatic battery cell will be produced in Thailand from raw materials and component parts in a fully automated production line. The raw materials (e.g., binders, solvents, additives, etc.) along with semi-finished and finished components (e.g., aluminum foil, copper foil, separator material, electrolyte, battery connectors, etc.) are all sourced from China.
According to your submission, the materials will arrive in Thailand in the form of material rolls, in powder form, or as liquids shipped in bulk containers. You state that the battery connectors, battery housing, aluminum foil, or copper foil may also be sourced domestically in Thailand. The manufacturing process begins in Thailand with milling and mixing the raw materials that will be used to produce the coating material for the electrodes of the battery cell.
The first coating material is for the anode electrode, which is prepared by dissolving a sodium carboxymethyl cellulose binder in an N-methyl-2-pyrrolidone solvent. Afterwards, graphite material is added to the solution and mixed into a homogenous slurry. A second slurry for the cathode electrode is created using lithium-ion phosphate, polyvinyl fluoride, and other materials. The slurries are then coated onto aluminum or copper foils that function as current collectors.
The coated foils are dried in an oven and then wound into semi-finished rolls. The rolls are fed into a calendaring press that works the coated foil to the required thickness and increases the density and binding strength between the active material and current collector. Using a laser cutting process, the rolls are slit into strips that are then cut to size and shape, which includes forming the electrode tabs.
Next comes winding, a process that is described as alternately stacking electrode sheets and separators to form a jelly roll structure. The electrode tabs are grouped together and welded to the battery cover. The jelly roll is wrapped with mylar and placed inside an aluminum battery case, which is sealed by laser welding the cover to the case.
At this point, the cell is ready for activation, a process that involves pre-charging the battery cell at a low charging speed to form a solid electrolyte interface, heating the cell in a vacuum chamber to prevent water from reacting with the electrolyte, and pumping electrolyte into the cell. Lastly, each cell is tested and sealed, which involves using a high temperature aging process to accelerate the absorption of electrolyte, introducing a second injection of electrolyte, and hermetically sealing the cell.
The text above is an excerpt. The official ruling, with its letterhead, signature and any attachments, is on CBP CROSS (N350953).