The country of origin of textured silicon wafers
No revocation or modification of this ruling appears in the Customs Bulletin issues read here (Nov 6, 2024 through Nov 18, 2026), where CBP publishes most such actions. That is not confirmation that the ruling is still in effect. Confirm its status with CBP before relying on it (ruling on CBP CROSS).
Key passages, quoted from the ruling
- As such, the country of origin of the textured silicon wafers will be Thailand.
Ruling text
In your letter dated October 30, 2025, you requested a country of origin ruling on textured silicon wafers on behalf of Canadian Solar International Limited. The items concerned are referred to as textured silicon wafers that will be used in the manufacture of solar cells.
Silicon ingots from China or various other countries of origin (Egypt, France, Germany, India, Indonesia, Laos, Malaysia, Nigeria, Norway, Romania, Spain, Turkey, the UAE, Vietnam, Taiwan, Thailand, and the USA), with a chemical composition of 99.99% silicon (Si) are sent to Thailand, where they are manufactured into textured silicon wafers through the process outlined below. The textured silicon wafers are then shipped to the United States to be processed into solar cells.
The processing that takes place in Thailand incudes the following: The Wire Saw Cutting Process: The wafer cutting process begins when an ingot of silicon is cut into rectangular bricks. The bricks are then glued and mounted onto a holder and placed into a wire saw. The bricks are then cut into individual wafers. The wire spacing and the wire diameter determine the wafer thickness, typically 150 micrometers.
The Gettering Process: The gettering process removes metallic impurities and is an integral part of the wafer fabrication process. It is composed of two major parts, including a wet chemical process to remove saw damage and a high temperature gettering process to reduce metallic impurities. The wafers are bulk-doped with phosphorus (~0.01–0.1 ppm) for a negative-type conductivity attribute.
As a result of the Thailand manufacturing process, the phosphorus doping profile measured by ECV (electrochemical capacitance-voltage) contains a high surface doping concentration of 1E19 cm-3, which is four orders of magnitude compared with the base phosphorus doping (1~4E15 cm-3).
Phosphorus (the negative dopant) is added during both ingot growth and phosphorous gettering diffusion (Thailand), while Boron (the positive dopant), will be imparted later in the nanocrystalline silicon layer in the Unites States, during solar cell manufacturing, to form the P/N junction. The Texturing Process: Texturing the surface of wafers is essential in the production of high-efficiency silicon.
Texturing uses chemicals to create pyramids on the wafer's surface, lowering reflectivity and increasing the amount of light that can be trapped. The Oxidization Process: Thermal oxidation of silicon wafers is a process in which a layer of silicon dioxide is formed on the surface of a silicon wafer under high temperatures. The Oxidization Removal Process & Polishing: The rear side of the silicon wafer is polished to enhance internal light reflection, which can largely enhance the light conversion efficiency.
One side of the oxide layers is removed by HF solution while the other side is left to act as a protection layer in the polishing step. The Inspection and Packaging Process: The inspection process ensures that silicon wafers are free of defects, including cracks, edge chips, and breakage.
The text above is an excerpt. The official ruling, with its letterhead, signature and any attachments, is on CBP CROSS (N355523).