No revocation or modification of this ruling appears in the Customs Bulletin issues read here (Nov 6, 2024 through Nov 18, 2026), where CBP publishes most such actions. That is not confirmation that the ruling is still in effect. Confirm its status with CBP before relying on it (ruling on CBP CROSS).
Ruling text
In your letter dated August 27, 2026, on behalf of Cleansky Co., LTD, you requested a country of origin and marking ruling on a ceramic honeycomb catalyst. The product under consideration is a ceramic honeycomb catalyst consisting of a ceramic honeycomb substrate and a washcoat layer (catalyst coating layer) impregnated with precious metals. At the time of import, it is a fully finished catalyst capable of performing its catalytic functions.
After importation, it will be assembled into a catalytic converter in the United States.
The manufacturing process for the ceramic honeycomb catalyst is described as follows: US-origin alumina (Model: MI-386 SP), Germany-origin alumina (Model: Sba-200), China-origin oxygen storage component (OSC) (Model: Actalys-063), Japan-origin barium hydroxide, South Korea-origin acetic acid, China-origin octyl alcohol, Malaysia-origin monoethanolamine (MEA), and South Korea-origin palladium nitrate, rhodium nitrate, and distilled water are weighed to prepare a catalyst coating solution.
The distilled water, acetic acid, barium hydroxide, alumina (MI-386 SP and Sba-200), and OSC are added for the primary mixing. Subsequently, palladium nitrate and rhodium nitrate are added along with MEA, which serves to maintain the precious metal precursors in a stable complex state. A final mixing is then performed to complete the catalyst coating solution.
The pH, solid content, and particle size of the completed catalyst coating solution are measured, and if they meet the standard values, the coating process proceeds. Before coating, the weight of the China-origin ceramic honeycomb is measured. The ceramic honeycomb is then coated with the catalyst coating solution using a dip-coating method.
Following this, excess catalyst coating solution is removed via air blowing, and the weight is measured again to verify the exact amount of catalyst coating solution applied to the ceramic honeycomb. Once the coating is complete, the product is dried in a drying oven and then undergoes calcination in a furnace. The calcination process is conducted at temperatures of 450°C or higher. It removes impurities and nitrate components present in the washcoat.
The distilled water, acetic acid, octyl alcohol, and MEA are eliminated during the drying and calcination processes. The palladium nitrate and rhodium nitrate contained in the catalyst coating solution undergo chemical reactions through thermal decomposition and oxidation during the calcination process.
During this step, the nitrate components (NO3-) undergo thermal decomposition and are removed in the form of nitrogen dioxide (NO2) and oxygen (O2), while palladium and rhodium are converted into palladium oxide (PdO) and rhodium oxide (Rh2O3), respectively, becoming fixed onto the washcoat. The calcination process also enhances the adhesion between the ceramic honeycomb and the catalyst coating layer, preventing the catalyst from detaching during vehicle operation.
After the drying and calcination processes, the final weight of the ceramic honeycomb catalyst is measured to confirm the total catalyst coating amount, after which the product is packaged and shipped.